welding:
The welding process is an important process in the production of the steel space frame, and it must be carried out in strict accordance with the welding operation instructions. Minimize the residual stress caused by welding, and timely correct the deformation by means of flame heating.
A. When the steel pipe is welded with the sealing plate and the steel pipe, the groove shall be opened according to the requirements, and the groove angle shall meet the requirements of the angle formed between the electrode and the groove surface to avoid unfusion and slag inclusion. In addition, the groove gap should be Large enough so that the electrode arc can reach the bottom of the groove and avoid insufficient penetration depth.
B. Avoid setting the welding seam to the middle of the rod when the steel pipe is butted.
C. Matters needing attention in welding operation:
a. During manual arc welding, the conveying range should not be too large, and multi-pass and multi-layer welding is used.
During the process, the weld bead or interlayer welding slag, slag inclusion, oxide, etc. should be strictly removed. Grinding wheel, steel can be used.
Tools such as wire brushes.
b. The same welding seam should be welded continuously and completed at one time.
c. For various weld joints, after the welding is completed, the slag and metal spatter on the surface of the weld should be cleaned up.
Check the appearance quality of the weld, and there must be no depression, weld bead, undercut, blowhole, lack of fusion, crack
and other defects exist.
d. After the butt weld is welded, ultrasonic flaw detection should be carried out after 24 hours.
Product detail pictures:
Related Product Guide:
Our firm sticks on the theory of "Quality will be the life in the enterprise, and status could be the soul of it" for Excellent quality Double Layer Grid Space Frame - Welding procedure of steel space frame – Puye , The product will supply to all over the world, such as: Uganda, Berlin, Madrid, Immediate and specialist after-sale service supplied by our consultant group has happy our buyers. Detailed Info and parameters from the merchandise will probably be sent to you for any thorough acknowledge. Free samples may be delivered and company check out to our corporation. n Morocco for negotiation is constantly welcome. Hope to get inquiries type you and construct a long-term co-operation partnership.
By Roberta from Munich - 2017.06.19 13:51
The company account manager has a wealth of industry knowledge and experience, he could provide appropriate program according our needs and speak English fluently.
By Cora from Cape Town - 2018.10.31 10:02